The easily cleavable planes of NdFeB magnets are the topic of discussion in this post.
Definition of Easily Cleavable Planes in NdFeB Magnets
The easily cleavable crystal planes of NdFeB magnets refer to the crystal planes in which the atoms are relatively loosely arranged and the interatomic bonding forces are relatively weak, making it easy for cleavage or slip to occur along these planes under external forces.

The presence of such planes causes cracks to propagate rapidly along the easily cleavable planes when the NdFeB magnet is subjected to external impact, thermal stress, or magnetostrictive stress, leading to brittle fracture of the material, which manifests as sudden fracture without obvious plastic deformation.
Impact of Easily Cleavable Planes on Magnetic Properties
| Magnetic Anisotropy: The easily cleavable planes of NdFeB magnets are closely related to magnetocrystalline anisotropy. The magnetization direction along the easily cleavable planes has the lowest energy, which enables the magnet to exhibit stronger magnetic anisotropy in the easy-axis direction.

| Grain Size and Magnetic Properties: The grain size of the easily cleavable planes has an important influence on magnetic properties. Fine grains (e.g., refined through additive manufacturing or heat treatment) can reduce the interaction between magnetic domains and improve the coercivity. However, excessively fine grains may lead to weakened magnetic anisotropy, so the grain size and magnetic properties need to be balanced through process optimization.
| Microstrain and Magnetic Property Degradation: Microstrain near the grain boundaries (such as lattice distortion) may be distributed along the easily cleavable planes, leading to a decrease in the magnetocrystalline anisotropy constant and the formation of “degradation zones,” which in turn reduce coercivity. This degradation effect can be alleviated by controlling microstrain or optimizing the grain boundary structure.
Relationship Between Easily Cleavable Planes and Brittleness in NdFeB Magnets
| Easily Cleavable Planes: The main phase of NdFeB magnets has a tetragonal crystal system. The atomic arrangement on the cleavage planes is relatively loose, and the interatomic bonding forces are relatively weak, making it easy for cleavage or slip to occur along these planes under external forces, leading to crack initiation and propagation.
| Brittle Behavior: Due to the presence of the easily cleavable planes, cracks tend to propagate rapidly along these planes when the NdFeB magnet is subjected to external impact, thermal stress, or magnetostrictive stress, resulting in brittle fracture of the material, characterized by sudden fracture without obvious plastic deformation.

Other Factors Affecting Brittleness
| Complexity of Crystal Structure: The crystal structure of NdFeB magnets is complex, with few slip systems and restricted dislocation movement, making it difficult to release stress through plastic deformation, which further aggravates the brittleness.

| Manufacturing Process: Magnets prepared by the powder metallurgy process contain micropores, defects, and residual stresses, which can serve as crack sources and reduce the toughness of the material.
| Grain Boundary Characteristics: Grain boundaries are weak links in the magnet. The Nd-rich phase and impurity elements at the grain boundaries can reduce the grain boundary bonding strength, making cracks easier to propagate along the grain boundaries, leading to intergranular fracture.

Magnets Manufacturer
At Tengye, we’re thrilled to be early participants in your new projects. Our passion for magnets extends from material selection and design optimization to providing magnetic solutions. We hope to bring our knowledge and experience to the forefront by actively engaging in your upcoming projects. Work with our magnet experts to get the right magnet solution.