The “plastic liquefaction” of the grain boundary phase in NdFeB magnets mainly occurs during processes such as hot deformation, high-temperature sintering, and grain boundary diffusion. Its core lies in the liquefaction of the low-melting-point grain boundary phase at elevated temperatures, which triggers grain boundary sliding, grain rearrangement, or promotes elemental diffusion, exerting a decisive influence on the microstructure and magnetic properties of the magnet.
Principle of “Plastic Liquefaction” of the Grain Boundary Phase
When the temperature reaches the melting point of the grain boundary phase, the grain boundary phase undergoes liquefaction, forming a liquid capillary network. The liquefied grain boundary phase acts as a “lubricant,” buffering the compressive stress at grain interfaces, reducing the deformation resistance of the grains, and promoting dissolution-precipitation diffusion creep of the grains.

Effects of “Plastic Liquefaction” of the Grain Boundary Phase
| Promoting grain rearrangement and texture formation: The flow of the liquid grain boundary phase causes sliding between grains. Under stress, the grains (such as Nd₂Fe₁₄B) tend to rotate to align parallel to the direction of pressure, achieving a preferred orientation of the grains, thereby reducing the formation of randomly oriented coarse-grained regions.

| Promoting and suppressing grain growth: The flow of the liquid phase buffers the stress at grain interfaces. If the liquid phase segregates heavily at the interfaces, it buffers the compressive stress, causing random grain growth and the formation of coarse-grained regions; however, by regulating the grain boundaries to achieve a uniform distribution of the liquid phase, excessive grain growth and the formation of coarse-grained regions can be suppressed, preserving fine grains.

| Promoting elemental diffusion: The liquid phase provides a “highway” for the rapid diffusion of elements (such as heavy rare earths Tb and Dy), promoting the diffusion of elements along the grain boundaries into the grain interiors, forming a core-shell structure.

| Effect on Magnetic Properties: The flow of the liquid phase provides a diffusion channel for the heavy rare earths introduced on the surface, achieving compositional regulation at the grain boundaries and an increase in coercivity. Meanwhile, the flow and uniform coating of the liquid phase can effectively isolate the grains, weaken the magnetic coupling between grains, suppress the nucleation of reverse magnetization domains, and also improve the coercivity of the magnet.
Regulation of “Plastic Liquefaction” of the Grain Boundary Phase
The degree of “plastic liquefaction” of the grain boundary phase, its flow behavior, and its distribution directly determine the microstructure and final magnetic properties of the magnet. Therefore, in actual processing, the “plastic liquefaction” process must be precisely controlled through the regulation of temperature, pressure, and composition (such as adding low-melting-point or high-melting-point phases).

Magnets Manufacturer
At Tengye, we’re thrilled to be early participants in your new projects. Our passion for magnets extends from material selection and design optimization to providing magnetic solutions. We hope to bring our knowledge and experience to the forefront by actively engaging in your upcoming projects. Work with our magnet experts to get the right magnet solution.