The magnetic properties of NdFeB permanent magnets are closely related to grain size. The subject of this paper is the ultra-fine grain / sub-micron grain control technology for Nd-Fe-B magnets.
Connotation of Ultra-Fine Grain / Sub-Micron Grain in NdFeB Magnets
The ultra-fine grain / sub-micron grain of NdFeB magnets refers to a state in which the grain size of the NdFeB magnet in its microstructure reaches the lower limit of the micron scale or even the nanoscale, characterized by extremely small grain sizes. This is the core microstructural feature enabling Nd-Fe-B materials to achieve high performance (especially high coercivity).

Methods for Controlling Ultra-Fine Grain / Sub-Micron Grain
Compositional Regulation
| Adding grain refiners: Adding high-melting-point elements (such as niobium Nb, zirconium Zr) or low-melting-point elements (such as gallium Ga) to the alloy formulation. During rapid solidification or sintering, these elements can “pin” the grain boundaries, suppress grain growth, and simultaneously optimize the intergranular phase, achieving sub-micron grain refinement.

| Optimizing the grain boundary phase: By optimizing the grain boundary phase to improve ultra-fine grain / sub-micron grain boundary continuity and reduce ferromagnetic coupling between grains, the loss of intrinsic coercivity can be reduced while refining the grains.

Powder Refinement
| Rapid cooling process: Spraying the molten alloy onto a high-speed rotating cooling roll effectively suppresses the formation of coarse α-Fe phase and refines the grains to the micron scale, providing fine-grained feedstock for subsequent powder production.
| Jet milling: Hydrogen decrepitation is used to crack the alloy into coarse powder, which is then ultra-finely pulverized by high-pressure gas flow (jet milling) to refine the powder. Using helium jet milling can further reduce the particle size and narrow the particle size distribution.

| Oxygen control and fine powder protection: During powder processing, the oxygen content must be strictly controlled to prevent oxidation of the fine powder from consuming the Nd-rich grain boundary phase, which would affect subsequent grain boundary repair and refinement effects.

Forming Control
| Pressureless sintering and low-temperature sintering: Using pressureless sintering (PLP) technology, pressing and sintering are carried out under a protective atmosphere, which reduces oxidation and suppresses abnormal grain growth; replacing high-temperature sintering with low-temperature sintering can slow down the grain growth tendency over time and maintain a fine-grained structure.
| Grain boundary infiltration: Optimizing the grain boundary structure so that the Nd-rich phase is uniformly distributed, thereby suppressing grain growth; combined with grain boundary diffusion (GBD) technology, heavy rare earths are diffused through the surface to optimize the grain boundaries, achieving a further increase in coercivity under fine-grained conditions.

Magnets Manufacturer
At Tengye, we’re thrilled to be early participants in your new projects. Our passion for magnets extends from material selection and design optimization to providing magnetic solutions. We hope to bring our knowledge and experience to the forefront by actively engaging in your upcoming projects. Work with our magnet experts to get the right magnet solution.